Pre-alloyed Powder: SFN-10

Pre-alloyed Powder: SFN-10


    Iron - copper - nickel - tin pre-alloyed powder, the average particle size of the powder is 2000 mesh, D50 is 4.8-6.8 microns. the section is shallow dimple honeycomb structure, the fineness is similar to that of cobalt powder.


  • Awesome Image High strength and hardnessd
  • Awesome Image Cobalt powder properties can be partially substituted, better sharpness after replacement
  • Awesome Image The strength and hardness curves in the temperature range of 700-900℃ are stable close to cobalt powder


Data


Grade Fe(%) Cu(%) Ni(%) Sn(%) Hardness Bending Strength
SFN-10 Main Component 18 2 2 Max: 109 HRB Max: 1459 MPa